| Customization: | Available |
|---|---|
| Processing Object: | Metal |
| Molding Style: | Forging |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
| Packaging Details: | Export standard package or according to customer requirement |
| Delivery Detail: | 30~60days according to various quantity |
| Name | Technique | Material | Dia/mm | Wall thickness |
Length/mm |
| Forging shaft | Forging+turning+grinding | alloy steel carbon steel stainless steel |
200-800 | ---- | 500-20000 |
| Hollow shaft | Forging+drilling+turning | 150-800 | ≥15mm | ≤17000 | |
| Shaft sleeve | Forge+drill & bore+turning +milling | 400-700 | ≥15mm | ≤18000 | |
| Large bolt | Rolled/forge+turning+threading | 300-800 | ---- | ≤17000 | |
| Hydraulic cylinder | Forging+drill & bore+ turning | 300-2000 | ≥10mm | ≤10000 | |
| Other parts in deep-hole | Forge+ drill & bore+turning+mill | 300-2000 | ---- | ≤20000 |
| Item | Process | Facility | Inspection items |
Standard |
| 01 |
Steel material inspection |
Chemical composition (EF+LF+VD) |
Material standard | |
| surface | Ingot inspection specification |
|||
| Ingot type and weight | Material standard | |||
| 02 |
Material store |
Division put | warehouse management | |
| 1 |
Heat | Heat furnace | Temperature/Time | Heating process specification Forging production procedure |
| 2 ↓ |
Forging | Press | Reduction ratio,forging temperature,deformation, Surface and dimensions |
Forging process card Forging procedure |
| 3 ↓ |
Heat treatment | heat treatment furnace |
heat treatment charts | 1st heat-treatment card Forging procedure |
| 4 ↓ |
Rough inspection |
Dimensions, apperance, Mark |
Inspection specification Forging procedure |
|
| 5 ↓ |
Rough UT | UT equipment | Single defect, concentrated Defects bottom wave attenuation |
UT standard or customer's technical requirements |
| 6 ↓ |
Saw cutting | Saw machine | Dimension | IQC and forging |
| 7 ↓ |
rough turning | turning-lathe | Dimension,appearance | Rough machining drawing |
| 8 ↓ |
UT | UT equipment | Single defect, concentrated defects bottom wave attenuation |
UT standard or customer's technical requirements |
| 9 ↓ |
Q+T heat treatment |
heat treatment furnace |
heat treatment charts | Heating process specification |
| 10 ↓ |
Sampling or machining | machining tool | rough machining drawing sampling drawing |
sample machining drawing |
| 11 ↓ |
mechanical property test |
tensile testing machine/ impact testing machine |
ambient temperature,humidity, Test temp.Sample dimension, test method |
Standard technical specification |
| 12 ↓ |
finish machining |
machining tool |
Dimension,appearance | finish machining drawing |
| 13 ↓ |
UT | UT equipment | Single defect, concentrated Defects bottom wave attenuation |
UT standard or customer's technical requirements |
| 14 ↓ |
MT | MT equipment | Magnetic particle indication |
Test standard or Technical requirements |
| 15 ↓ |
Mark | Steel seal | marking content | Product standard Technical requirements Forging process |
| 16 ↓ |
Final inspection |
Appearance, dimension, mark acceptance inspection |
Product inspection specification Product standard P.O. |
|
| 17 | Protection/ package |
Blasting Blasting equipment |
appearance coating thickness |
Product standard Technical requirements |